Home
/
/
Hot-Dip Galvanized, Aluminum-Zinc Coated, and Zinc-Aluminum-Magnesium Coated Steel Sheets

Hot-Dip Galvanized, Aluminum-Zinc Coated, and Zinc-Aluminum-Magnesium Coated Steel Sheets

Hot-Dip Galvanized, Galvalume (Al-Zn), and Zinc-Aluminum-Magnesium Steel Sheets
Hot-Dip Galvanized (GI), Galvalume (GL), and Zinc-Aluminum-Magnesium (ZAM) represent the current mainstream hot-dip anti-corrosion steel sheets. Their core difference lies in the composition of their coatings, which determines their corrosion resistance, self-healing capabilities, cost, and applicable scenarios.
I. Core Introduction to the Three Types of Steel Sheets
1. Hot-Dip Galvanized Steel Sheet (GI, Pure Zinc Coating)
Coating Composition: Pure zinc (Zn ≥ 99.9%), applied via a hot-dip process.
Appearance: Silvery-white; features large, coarse zinc spangles; prone to developing “white rust.”
Anti-Corrosion Principle: Zinc acts as a sacrificial anode to protect the steel sheet; corrosion is delayed through the gradual consumption of the zinc layer.
Core Performance
Corrosion Resistance: Withstands approximately 500–1000 hours in salt spray tests; expected service life in standard environments is 5–10 years.
Processing: Exhibits good ductility, is easy to weld, and offers the lowest cost among the three.
Disadvantages: Cut edges and scratches are prone to rusting; lacks self-healing properties; has a shorter service life in humid or salt-spray environments.
Applicable Scenarios: Dry indoor environments, short-term outdoor applications, general construction, internal components of home appliances, and projects with limited budgets.

For outdoor use, a zinc coating weight of ≥ 200 g/m² is recommended.

2. Galvalume Steel Sheet (GL, 55% Aluminum-Zinc Alloy)
Coating Composition: 55% Aluminum + 43.5% Zinc + 1.5% Silicon, applied via hot-dip process.
Appearance: Light silvery-gray; features fine, uniform zinc spangles; possesses a soft, matte luster.
Anti-Corrosion Principle: Aluminum forms a dense oxide film that acts as a barrier against corrosion, while zinc provides a secondary layer of protection through sacrificial anodization.
Core Performance
Corrosion Resistance: Withstands 2000–3000 hours in salt spray tests (2 to 6 times longer than hot-dip galvanized steel); expected service life in standard environments is 15–30 years.
High-Temperature Resistance: Capable of withstanding temperatures up to 315°C; demonstrates strong resistance to atmospheric corrosion and humidity.
Disadvantages: Offers weak protection at cut edges; weldability is average; exhibits poor resistance to alkaline substances.
Applicable Scenarios: General outdoor construction, industrial plant buildings, home appliance casings, and general industrial environments.

For outdoor use, a zinc coating weight of ≥ 200 g/m² is recommended. 3. Zinc-Aluminum-Magnesium Coated Steel (ZAM; Ternary Zn-Al-Mg Alloy)
Coating Composition: Mainstream 91% Zinc + 6% Aluminum + 3% Magnesium (High-magnesium versions contain 5%–6% Mg); utilizes an upgraded hot-dip coating process.
Appearance: Matte silver-gray finish with no visible spangles (zinc crystals), offering a premium aesthetic.
Corrosion Protection Mechanism: Combines zinc’s sacrificial anode effect, aluminum’s barrier effect, and magnesium’s role in promoting the formation of a dense, composite passivation film; features self-healing capabilities for cut edges and scratches.
Core Performance
Corrosion Resistance: Withstands 5,000–8,000 hours in salt spray testing—5 to 20 times the resistance of standard hot-dip galvanized steel—offering a service life of 25+ years in harsh environments.
Self-Healing: Automatically forms a protective film at cut edges or damaged areas, preventing the spread of rust and corrosion.
Processability: Resists cracking during bending or stamping; exhibits strong coating adhesion and excellent weldability.
Disadvantages: Highest cost among the options.
Applicable Scenarios: Marine/coastal environments, areas with industrial pollution, high-humidity conditions, high-salt-spray environments, photovoltaic mounting systems, livestock farming facilities, and long-term maintenance-free engineering projects.

For outdoor applications, a zinc coating weight of ≥150 g/m² is recommended.

II. Core Performance Comparison (At a Glance)
Table
Comparison Item | Hot-Dip Galvanized (GI) | Galvalume (GL) | Zinc-Aluminum-Magnesium (ZAM)
Coating Composition | Pure Zinc (≥99.9%) | 55% Al + 43.5% Zn + 1.5% Si | 91% Zn + 6% Al + 3% Mg (Mainstream)
Salt Spray Lifetime | 500–1,000 hours | 2,000–3,000 hours | 5,000–8,000+ hours
Corrosion Resistance Factor | 1x | 2–6x | 5–20x
Self-Healing Capability | None | Weak | Strong (Self-healing at cut edges/scratches)
High-Temperature Resistance | 200°C | 315°C | 300°C
Weldability | Good | Fair | Good
Cost | Lowest | Medium | Highest
Typical Service Life | 5–10 years | 15–30 years | 25–40 years

滚动至顶部

We use cookies and other technologies.

This website uses cookies and similar functions to process end device information and personal data. The processing serves the integration of content, external services and elements of third parties, statistical analysis/measurement, personalized advertising (Google Remarketing) and the integration of social media. Depending on the function, data may be passed on to third parties in the process and to third parties in countries where there is no adequate level of data protection and is processed by them, e.g. the USA. Your consent is always voluntary, not required for the use of our website and can be rejected or revoked at any time on our site.